This search combines search strings from the content search (i.e. "Full Text", "Author", "Title", "Abstract", or "Keywords") with "Article Type" and "Publication Date Range" using the AND operator.
Beilstein J. Nanotechnol. 2016, 7, 1709–1717, doi:10.3762/bjnano.7.163
Figure 1: SEM top view of the obtained porous alumina oxide at different magnification a) 20000×, b) 100000×.
Figure 2: Deposited mass of Ni and of Ni–Fe as a function of the deposition time. Alumina thickness (HPA) is ...
Figure 3: SEM cross-sectional views of the alumina template after galvanostatic dc deposition of Ni–Fe (a, b,...
Figure 4: XRD pattern for Ni NWs in alumina template with HPA of 65 μm and a current density of 3 mA·cm−2, de...
Figure 5: XRD pattern of Ni–Fe NWs inside the alumina template with HPA of 50 μm and a current density 3 mA·cm...
Figure 6: Magnetization as a function of the temperature for Ni NWs fabricated in the alumina template (HPA =...
Figure 7: Magnetization as a function of the temperature for Ni–Fe NWs fabricated in the alumina template (a)...